Material selection we offer
Material |
Density(g/cm3) |
Pull strength (MPA) |
Yield strength (MPA) |
Elongation (%) |
Hardness |
Heat treatment method |
4605
(Heat Treated)
|
>7.5 |
1,655 |
1,480 |
2 |
HRC 46-52 |
Oil quenching and tempering |
Fe8Ni
(Heat Treated)
|
>7.5 |
1,750 |
1,450 |
5 |
HRC 47-53 |
Gas/oil quenching and tempering |
316L |
>7.5 |
500 |
350 |
40 |
HRC 50-60 |
No heat treatment |
420
(Heat Treated)
|
>7.3 |
1,200 |
1,000 |
1~2 |
HRC 40-48 |
Gas/oil quenching and tempering |
440C
(Heat Treated)
|
>7.5 |
950 |
--- |
1~2 |
HRC 56-62
(Hv0.1>650) |
Gas/oil quenching and tempering |
17-4PH
(Heat Treated)
|
>7.5 |
1,190 |
1,050 |
5 |
HRC 31-36 |
Solid solution and precipitation |
More
material
options |
Any other questions, please contact us. |